The polymerization shrinkage of composite resins.
The polymerization shrinkage of composite resins.
J. Rees,P. Jacobsen
1989 · DOI: 10.1016/0109-5641(89)90092-4
Dental Materials · 126 Citations
TLDR
Six materials were investigated: Aurafill, Silar, Concise, Heliomolar, P-30, and Occlusin, and results ranged from 0.9 to 2.24 volume percent, with current concern for industrial hygiene, the water-filled dilatometer may have advantages.