Abstract
Clay soils, which possess expansive characteristics, are known to be problematic in construction due to their low
strength, poor load-carrying capacity, and high shrink-swell potential. These clay soils undergo substantial volume changesdue to variations in moisture content, which can cause instabilities in structures such as foundations, pavements, and othercivil constructions. Ordinary Portland Cement (OPC) stabilization has proven to be a popular solution. However, the highcost of production makes it very expensive and less affordable. Therefore, alternative methods, which are cost-effective andmore sustainable, require investigation. This paper has investigated the behavior of expansive clay soil stabilized underSorghum Husk Ash (SHA)-Blended cement with the focus on its Atterberg limits, compaction properties, and CaliforniaBearing Ratio (CBR). Soil samples were collected from Nkondi ward in Tharaka Nithi County, Kenya, and sorghum huskswere sourced from Mwanyani location, Tharaka Nithi county. The samples were calcined and mixed with 40% cement tomake blended cement composed of clinker (40%), calcined clay (20%), sorghum husk ash (20%), limestone (15%), andgypsum (5%). Tests were conducted in the laboratory by using AASHTO T-180 standards. This study investigated theengineering properties of a soil sample through particle size distribution, Atterberg limits, compaction, California BearingRatio (CBR), and swell potential tests, following BS 1377 and AASHTO standards. The particle size distribution showedthat 62.6% of the fines passed through the 0.075 mm sieve, indicating a predominance of fine particles. Atterberg limits gavea liquid limit of 44.3%, a plastic limit of 28.1%, and a plasticity index of 16.2%, confirming measurable plasticity.Compaction results using AASHTO T-180 revealed a maximum dry density of 1.593 g/cm3 at an optimum moisture contentof 21.7%. The CBR test values increased with compaction effort, ranging from 23.8% at low compaction to 88.7% at highcompaction, while swell potential decreased from 0.65% to 0.13%. According to the study, sorghum husk ash-modifiedcement successfully enhanced the engineering properties of expansive clay by improving compaction properties, increasingbearing capacity, and preventing material swelling. This SHA-Blended cement can offer an economical and sustainablesubstitute to OPC in soil stabilization.